| Brand Name: | Jinxi Pipe |
| Model Number: | Alloy Steel Pipe |
| MOQ: | 1 |
| Price: | 1500 USD/TON |
| Payment Terms: | L/C,D/A,D/P,T/T,Western Union,MoneyGram |
| Supply Ability: | 100000 |
ASTM A213 T36 Alloy Steel Tube High-Temperature Pressure Tubing
Specification
ASTM A213 T36 alloy steel tube is specified for high-temperature applications such as boilers, superheaters, and heat exchangers. These tubes are known for their high-temperature strength, corrosion resistance, and durability, and are typically manufactured with chromium and molybdenum additions. They must meet specific heat treatment and mechanical property requirements defined by the ASTM A213 standard.
| American Standard | Standard Name |
| A213 / A213M | Seamless Ferritic and Austenitic Alloy-steel Boiler,Superheater and Heat-Exchanger Tubes |
![]()
ASTM A213 T36 Alloy Steel Pipe Chemical Composition
Sources American Standard A213 / A213M TABLE 1 Chemical Composition Limits, % , for Low Alloy Steel
| Grade | UNS Designation |
C | Mn | P | S | Si | Ni | Cr | Mo | V | Nb | N | Al | Others |
| T36 | K21001 | 0.10-0.17 | 0.80-1.20 | 0.03 | 0.025 | 0.25-0.50 | 1.00-1.30 | 0.3 | 0.25-0.50 | 0.02 | 0.015-0.045 | 0.02 | 0.05 | Cu 0.50-0.80 |
ASTM A213 T36 Alloy Steel Pipe Mechanical Properties
Sources American Standard A213 / A213M TABLE 4 Tensile and Hardness Requirements
| Grade Low Aloy Steels: |
UNS Designation |
TensileStrength. min, ksi [MPa] |
Yield Strength ,min, ksi [MPa] |
Elongationin 2 in. or 50 mm. min, %B.C |
HardnessA | |
| Brinell/Vickers | Rockwell | |||||
| T36 Class 1 | K21001 | 90 [620] | 64 [440] | 15 | 250 HBW/265 HV | 25 HRC |
| T36 Class 2 | K21001 | 95.5 [660] | 66.5 [460] | 15 | 250 HBW/ 265 HV | 25 HRC |
ASTM A213 T36 Alloy Steel Pipe Heat Treatment
Sources American Standard A213 / A213M TABLE 3 Heat Treatment and Grain Size Requirements A
| Grade Ferritic Alloy Steels |
UNS Designation |
Heat Treatment Type | Austenitizing/Solution Treatment StabilizingTemperature,min or range °F [°C] |
Cooling Media | Subcritical Annealingor TemperingTemperature,min or range °F [°C] |
| T36 | K21001 | normalize and temper | 1650[900] | E | 1100[595] |
| E Accelerated air cooling or liquid quenching shall be permitted for Class 2. | |||||
ASTM A213 T36 Alloy Steel Pipe Manufacturing Proces
![]()
ASTM A213 T36 Alloy Steel Pipe Application
ASTM A213 T36 Alloy Steel Pipe Packing & Loading
a. 1/2"-2"Plain end with black oil paint, caps both ends, bundles with loading belt.
b. 2"-4"Beveled end with black oil paint, caps both ends, bundles with loading belt.
c. 10"-20"Beveled end with black oil paint, caps both ends, loose packed in to container.
![]()
→Alloy Steel Pipes is transported in containers
![]()