| Brand Name: | Jinxi Pipe |
| Model Number: | Alloy Steel Pipe |
| MOQ: | 1 |
| Price: | 1500 USD/TON |
| Payment Terms: | L/C,D/A,D/P,T/T,Western Union,MoneyGram |
| Supply Ability: | 100000 |
ASTM A213 T24 Alloy Steel Tube For Water Wall Panels in Boilers
Specification
ASTM A213 T24 alloy steel tube is designed for high-temperature applications like boilers, superheaters, and heat exchangers. It is a chrome-moly tube, meaning it contains chromium and molybdenum, with a specific composition of about 2.20-2.60% chromium and 0.90-1.10% molybdenum. Key characteristics include good high-temperature strength, oxidation resistance, and durability.
| American Standard | Standard Name |
| A213 / A213M | Seamless Ferritic and Austenitic Alloy-steel Boiler,Superheater and Heat-Exchanger Tubes |
![]()
ASTM A213 T24 Alloy Steel Pipe Chemical Composition
Sources American Standard A213 / A213M TABLE 1 Chemical Composition Limits, % , for Low Alloy Steel
| Grade | UNS Designation |
C | Mn | P | S | Si | Cr | Mo | V | B | N | Al | Others |
| T24 | K30736 | 0.05-0.10 | 0.30-0.70 | 0.02 | 0.01 | 0.15-0.45 | 2.20-2.60 | 0.90-1.10 | 0.2-0.3 | 0.0015-0.007 | 0.012 | 0.02 | Ti 0.06-0.10 |
ASTM A213 T24 Alloy Steel Pipe Mechanical Properties
Sources American Standard A213 / A213M TABLE 4 Tensile and Hardness Requirements
| Grade Low Aloy Steels: |
UNS Designation |
TensileStrength. min, ksi [MPa] |
Yield Strength ,min, ksi [MPa] |
Elongationin 2 in. or 50 mm. min, %B.C |
HardnessA | |
| Brinell/Vickers | Rockwell | |||||
| T24 | K30736 | 85 [585] | 60 [415] | 20 | 250 HBW/265 HV | 25 HRC |
ASTM A213 T24 Alloy Steel Pipe Heat Treatment
Sources American Standard A213 / A213M TABLE 3 Heat Treatment and Grain Size Requirements A
| Grade Ferritic Alloy Steels |
UNS Designation |
Heat Treatment Type | Austenitizing/Solution Treatment StabilizingTemperature,min or range °F [°C] |
Cooling Media | Subcritical Annealingor TemperingTemperature,min or range °F [°C] |
| T24 | K30736 | normalize and temper | 1800-1870[980-1020] | D | 1350-1420[730-770] |
| D Accelerated cooling from the normalizing temperature shall be permitted for section thicknesses greater than 3 in. [75 mm]. | |||||
ASTM A213 T24 Alloy Steel Pipe Manufacturing Proces
![]()
ASTM A213 T24 Alloy Steel Pipe Application
ASTM A213 T24 Alloy Steel Pipe Packing & Loading
a. 1/2"-2"Plain end with black oil paint, caps both ends, bundles with loading belt.
b. 2"-4"Beveled end with black oil paint, caps both ends, bundles with loading belt.
c. 10"-20"Beveled end with black oil paint, caps both ends, loose packed in to container.
![]()
→Alloy Steel Pipes is transported in containers
![]()